Can anyone steer me to a company that can measure the surface finish on .6 module brass worms (ie. 6 mm diameter) Any companies I have tried have told me that the parts are too small for their equipment.

Any suggestions would be appreciated
 
Replies continue below

Recommended for you

You might try a company with optical or laser microscopes that also have software for computing surface roughness. Michigan Metrology may be an option.
 
Can't you use visual methods to confirm your
surface finish? How fine a surface do you need?
 