MEASURING RETAINED AUSTENITE.

Status
Not open for further replies.

ibf

Mining
Feb 25, 2004
83
HELLOW !

Is there a portable instrument that allows me to measure retained austenite "in-situ", or the only possible way is via the traditional lab sources such as : X-ray , .... and others ?

Thank you.



 
Replies continue below

Recommended for you

Barkhousen Effect devices will allow you to do this, and I believe some are portable. But, the information is qualitative/semi quantitative. How accurate do you need to be?
 
After getting back to the office and reviewing my literature, I find that portable XRD equipment is available. Try American Stress Technologies at
 
Semi quantitative would do. Could you give me a web site and/or a contact on the Co. that supplies such an equipment ?

 
Thank you very much swall.
 