I am looking for a novel way to measure the dry density of tailings as it desaturates due to an evaporation potential.
I am trying to establish the relationship between moisture content and dry density. As a tailings settles out from the slurry it remains saturated and so working out the dry density and moisture content is simple. (It can be assumed the relationship follows the zero air voids line - any comments?)
However at a specific moisture content the sample starts to desaturate. At this point it becomes difficult to determine the dry density as one needs to measure both volume and mass. Further complicating the matter is that the sample cracks which makes determining the volume harder.
Any suggestions as to test methods or devices to measure the dry density post saturation?
I am trying to establish the relationship between moisture content and dry density. As a tailings settles out from the slurry it remains saturated and so working out the dry density and moisture content is simple. (It can be assumed the relationship follows the zero air voids line - any comments?)
However at a specific moisture content the sample starts to desaturate. At this point it becomes difficult to determine the dry density as one needs to measure both volume and mass. Further complicating the matter is that the sample cracks which makes determining the volume harder.
Any suggestions as to test methods or devices to measure the dry density post saturation?