Aug 9, 2006 #2 EdStainless Materials Joined May 20, 2004 Messages 16,384 Location Waukesha WI USA Usually disolved gasses are measured by taking a sample and flashing the gass off. You might use pH and calculate based on the temp and dissociation coef. = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote