Jul 21, 2006 #1 kevlar49 Materials Joined Jun 1, 2006 Messages 287 Location US Are there any special rules for determining the MDMT for alky reactors/contactors or can I just apply the rules of ASME VIII UCS-66?
Are there any special rules for determining the MDMT for alky reactors/contactors or can I just apply the rules of ASME VIII UCS-66?
Jul 21, 2006 #2 roker Chemical Joined Jun 23, 2004 Messages 198 Location IL hello, the minimum operating temperature will be reached if the pressure vessel is opened to the atmosphere, on this calculated temperature a design margin should be added. regards, roker Upvote 0 Downvote
hello, the minimum operating temperature will be reached if the pressure vessel is opened to the atmosphere, on this calculated temperature a design margin should be added. regards, roker
Jul 21, 2006 #3 jte Mechanical Joined Apr 8, 2002 Messages 2,357 Location US This is really more of a question for forum794 but as far as I know, VIII-1 does not require anything beyond UCS-66. jt Upvote 0 Downvote
This is really more of a question for forum794 but as far as I know, VIII-1 does not require anything beyond UCS-66. jt