Dear respected experts.
I would like to inquire about the following problem.
I have a vessel with MDMT -46 deg C CS Carbon steel
PQR only specifies impact test at -45 deg C. (only 1 deg C difference)
I wonder if PQR is acceptable to be used on the vessel.
Is there some provisions in the ASME code that allows it?
Thanks in advance for your reply.
Best regards,
Genetix
ME/Petroluem
I would like to inquire about the following problem.
I have a vessel with MDMT -46 deg C CS Carbon steel
PQR only specifies impact test at -45 deg C. (only 1 deg C difference)
I wonder if PQR is acceptable to be used on the vessel.
Is there some provisions in the ASME code that allows it?
Thanks in advance for your reply.
Best regards,
Genetix
ME/Petroluem