Here below is the Visual Inspection Acceptance Criteria as per AWS D1.1 for Statically loaded non tubular connections (Table 6.1)
(8) Porosity
(A) CJP groove welds in butt joints transverse to the direction of computed tensile stress
shall have no visible piping porosity. For all other groove welds and for fillet welds, the
sum of the visible piping porosity 1/32 in [1 mm] or greater in diameter shall not exceed
3/8 in [10 mm] in any linear inch of weld and shall not exceed 3/4 in [20 mm] in any
12 in [300 mm] length of weld
Questions:
For fillet welds which should be the maximun diameter of piping porosity?
Always talking about "piping porosity" , there is not other kind of porosity to be evaluated?
Any input will be appreciated.
(8) Porosity
(A) CJP groove welds in butt joints transverse to the direction of computed tensile stress
shall have no visible piping porosity. For all other groove welds and for fillet welds, the
sum of the visible piping porosity 1/32 in [1 mm] or greater in diameter shall not exceed
3/8 in [10 mm] in any linear inch of weld and shall not exceed 3/4 in [20 mm] in any
12 in [300 mm] length of weld
Questions:
For fillet welds which should be the maximun diameter of piping porosity?
Always talking about "piping porosity" , there is not other kind of porosity to be evaluated?