Hi,
I was tensile testing welded sample of A 106 gr B, and the guage is reading an ultimate tensile streght of 87 to 90 ksi, in the spec, the minimum yield is 35 and the minimum tensile is 60 ksi, is the 87 ot 90 too high, is there a guide as to what the max should be or a range. The electrodes are E6010 root and hot pass and and 7010 cap for a 2" A106 B stick welding.
Thank you.
I was tensile testing welded sample of A 106 gr B, and the guage is reading an ultimate tensile streght of 87 to 90 ksi, in the spec, the minimum yield is 35 and the minimum tensile is 60 ksi, is the 87 ot 90 too high, is there a guide as to what the max should be or a range. The electrodes are E6010 root and hot pass and and 7010 cap for a 2" A106 B stick welding.
Thank you.