Can the material SA-106 Gr B be used by a manufacturer to manufacture a vessel according to ASME Section VIII DIV 2, If the design temperature is 750°F? Where can I find the maximum temperature for the material SA-106 GrB according to ASME Section VIII Div 2?
Thank You
 
Replies continue below

Recommended for you

ASME Section II, Part D, Table 5A. Temperature limit is 371 deg C (700 deg F). Refer also to note G13.