Good morning,

on ASME B31.1 Ed. 2016, A-335 P22 has the allowable stress shown in table until 1100°F.

Instead, on ASME BPVC II, D Ed. 2017, the material SA-335 P22 has the allowable stress shown in table until 1200°F.

What is the reason of this difference?

Thank you,

MM
 
Replies continue below

Recommended for you

The reason is two different groups of engineers developed these codes .....

What exactly are you building or evaluating or trying to do ?

MJCronin
Sr. Process Engineer
 
Dear Sr,

we are developing a boiler with reheater. The reheater header and nozzles (inside the casing)and the main pipe outside are in SA-335 P22. During start-up, when pressure is not yet built-up, the fluid may reach for little time (less than 5 minutes) a temperature of ~ 605°C (~ 1125°F).
While the portion inside the casing can theoretically withstand this condition (since the ASME section II D is listing allowable stress for P22 up to 1200°F), we do not know how to deal with the outer pipe, that falls under B31.1 (since the allowable stresses are listed only up to 1100°F)

Thank you in advance

MM
 
Different codes, different basis for allowable stresses. A B31.3 instructor once told me the difference between B31.1 and B31.3 allowables. He explained that, if I recall correctly ,that .... apart from the differences between the intended use/service of both codes, the environment surroundinig a plant, with respect to human occupancy, also was important. The likelihood of people living near a power plant (e.g. near urban areas), combined with the typical higher pressures and temperatures in power plants, make that the allowables are lower, providing a higher design margin (and thus some more inherent safety, if you like). B31.3 refineries are typically found more on chemical/refinery sites, where less human habitat or houses in a near vicinity are found, e.g. rural areas.
 
Rural areas like, oh, Houston :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Pardon my occasional bad choice of words, maybe it's semantics, but keep in mind Im Dutch ;-)
 
XL83NL said:
but keep in mind Im Dutch

You say it like it's a bad thing...

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
XL83NL :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
So, in your opinion is it possible to use A-335 P22 in B31.1, NBEP for very short period (~5 minutes during start-up) above 110°F?
 
If I’m not mistaken the limits of B31.1 may not be exceeded. So no
 