please advise the maximum pressure for hydrotest of piping spool which contains flange 150#
refer to ASME 16.5 for material carbon steel group 1.1 is about 19.2 bar (from table 2-1.1. SME 16.5)
can we go more than this limit pressure
 

Attachments

  • flange working pressure.png
    flange working pressure.png
    128.9 KB · Views: 5
Replies continue below

Recommended for you

dear all..
please advise the maximum pressure for hydrotest of piping spool which contains flange 150#
refer to ASME 16.5 for material carbon steel group 1.1 is about 19.2 bar (from table 2-1.1. SME 16.5)
can we go more than this limit pressure
Hydrotest pressure is 1.5 times maximum working pressure at 38C.

Flanges just become part of the piping system and subject to the piping design code for hydrotest. The flanges may be the limiting factor, it might be something else, pipe thickness, pressure vessel MAWP limit etc
 
Hi,
Consider this link and standards mentioned.
Pierre
 