So interested here to know what maximum bed joint thickness would be permitted before compressive strength of the mortar might be affected.
TMS 602-13/ACI 530.1-13 3.3.B Placing mortar and units indicates that a 3/8" (9.5mm)thick bed is anticipated/typical. 3.3.F Site tolerances indicates that the bed joints between courses may vary by +/- 1/8" (3.2mm).
All issues of coursing aside and not including the first mortar bed on top of the foundation.
Questions:
Is anybody aware of what mortar bed thickness greater than that indicated above would cause structural concern?
For dumb reasons, not ours, there is a coursing issue here. The trade is proposing a 33/64" or 13mm as the standard mortar bed depth.
Although it doesn't make me comfortable would this 13mm bed depth as a maximum be acceptable?
Not keen on letting a site tolerance become interpreted as the new spec.
Comments/Thoughts?
thank-you.
TMS 602-13/ACI 530.1-13 3.3.B Placing mortar and units indicates that a 3/8" (9.5mm)thick bed is anticipated/typical. 3.3.F Site tolerances indicates that the bed joints between courses may vary by +/- 1/8" (3.2mm).
All issues of coursing aside and not including the first mortar bed on top of the foundation.
Questions:
Is anybody aware of what mortar bed thickness greater than that indicated above would cause structural concern?
For dumb reasons, not ours, there is a coursing issue here. The trade is proposing a 33/64" or 13mm as the standard mortar bed depth.
Although it doesn't make me comfortable would this 13mm bed depth as a maximum be acceptable?
Not keen on letting a site tolerance become interpreted as the new spec.
Comments/Thoughts?