Bagman2524
Structural
I'm connecting a 1/8" thick tube to the bottom flange of I-beams varying in thickness from 1/4" to 7/16". Sec J2.2b of ASD states that the min weld thickness depends on the thicker of the 2 parts joined and is per table J2.4.
For the max size fillet weld it states that for material less than 1/4", the weld is not greater than the thickness of the material. Does this mean the thicker part also? or the thinner part? If it goes by the thinner part than my max weld would be 1/8", but for I-beams flanges above 1/4" thick, my min would be 3/16" (greater than the max).
For the max size fillet weld it states that for material less than 1/4", the weld is not greater than the thickness of the material. Does this mean the thicker part also? or the thinner part? If it goes by the thinner part than my max weld would be 1/8", but for I-beams flanges above 1/4" thick, my min would be 3/16" (greater than the max).