somebody known the Yield Strength of the C12L15?

Thanks in advance.

Chavacano
 
Replies continue below

Recommended for you

If you are referring to cold finished A.I.S.I. grade 1215 (UNS G12150), then it should have a yield strength of about 60,000 psi. But, you could have found that with a simple internet search. If you are referring to some other material, then you will have to be more specific.

Johnny Pellin
 
yes, that's correct I found it on internet.