guys, I need your suggestion on the materials selection for compressor caseing.
At the begining of the design, the minimum operating temperature is -2C and MDMT is -25C. The vendor proposed SA516-55 for the compressor casing.
Now, the minimum operating temperature of the compressor is -28C and MDMT is -45C. The vendor did not recommend SA516-55 for low temp and changed the materials to SA352 Gr.LCB.
To me, it looks like Impact tested SA516-55 can be used to -45C, which is also specified in API617.
My questions are:
(1) Can I use SA516-55. If not recommended, why?
(2) What is the differece between these two materials, when used at lower temperature.
Thanks.
At the begining of the design, the minimum operating temperature is -2C and MDMT is -25C. The vendor proposed SA516-55 for the compressor casing.
Now, the minimum operating temperature of the compressor is -28C and MDMT is -45C. The vendor did not recommend SA516-55 for low temp and changed the materials to SA352 Gr.LCB.
To me, it looks like Impact tested SA516-55 can be used to -45C, which is also specified in API617.
My questions are:
(1) Can I use SA516-55. If not recommended, why?
(2) What is the differece between these two materials, when used at lower temperature.
Thanks.