Hi,
I'm Xeros,
Crude has MgCl & CaCl and potential HCl is high.
So, i'm to apply "Monel claddig" for Crude Tower Top Section.
Howevere, Someone said to me that Monel is not suitable if ammonia is injected to pH control at Crude Tower overhead. The reason is that the stress corrosion cracking could be occur to Monel by injected Ammonia in abnormal operation.
is this right?
Generally, i have known that ammonia stress corrosion cracking could be occured to copper alloy. Monel is Nickel based alloy but has lots of copper (about 30%).
Could incoloy 825 be applied if above matter is true?
I think that incoloy 825 has a good resistance for hydrochloric acid and no problem for ammonia stress corrosion cracking.
Regards,
I'm Xeros,
Crude has MgCl & CaCl and potential HCl is high.
So, i'm to apply "Monel claddig" for Crude Tower Top Section.
Howevere, Someone said to me that Monel is not suitable if ammonia is injected to pH control at Crude Tower overhead. The reason is that the stress corrosion cracking could be occur to Monel by injected Ammonia in abnormal operation.
is this right?
Generally, i have known that ammonia stress corrosion cracking could be occured to copper alloy. Monel is Nickel based alloy but has lots of copper (about 30%).
Could incoloy 825 be applied if above matter is true?
I think that incoloy 825 has a good resistance for hydrochloric acid and no problem for ammonia stress corrosion cracking.
Regards,