I'm trying to determine the MAWP of a vessel based on burst testing using UG-101 P = B/4 X Smu X E /Smur. I have the burst test data, and I can find the minimum tensile strength of the vessel material, Smu(316L bar), but I do not have actual tensile data for the material that the burst test specimens were fabricated from. UG-101 allows an alternate calculation that uses Smur, the "maximum tensile strength of range of specification at room temperature". The specification for the 316L bar only lists the minimum tensile strength. Where do I find the "maximum tensile strength of range of specification at room temperature"?