Any recommendations of high strength (90 ksi or so) materials capable of withstanding 420,000 PPM (42 %) H2S and 8 % CO2 at 400 degrees F (bottom hole temperature) at 17,000 psi pressure (bottom hole pressure) for an oilfield downhole application? We typically use 4140 HT or 17-4 PH stainless at H900 condition for our downhole tools, but these will become hydrogen embrittled. Thanks in advance for any ideas!