Hi,
For the fabrication of low temp. material flanges, my company wants to substitute A350 LF2 by AISI 4130 forgings.
Is this acceptable?

Thanks to every one
 
Replies continue below

Recommended for you

Flanges for any pressure/temperature service application should fall under ASME B16.5 regardless. I would suggest you review ASME B16.5 for an appropriate material substitution.
 