I have been looking into some material problem we have in our pumps. We have a few specifications of material possibly for a part we use that can have up to 1500 PSI on it.
The current part is cast c90300 bronze. We have had cracking issues in this part.
We have looked into a competitor part and the material they use is C67300 brass or CS33500, and possibly UNS 34000.
I'm looking into the basics and I'm trying to keep it as simple as possible, what do you look into to know what makes it stronger for high pressure applications. I found that the C90300 has a much lower Tensile and Yield strength rating compared to the two other materials I specified. Is is this something I can use to deterime a new material?
I'm just one of the drafter / designers here at this company and we do not have a engineer at the time for this type of work right now and I'm looking to you guys for help the first time. I have tried to search these fourms and I hope I found the proper location for this.
Some things I've noted on these types of material and found, C67300 is a typically forged type of material or bar round. I could assume that forging could be a big help for strength in the area we have the cracking issues at high pressure. And, is there possibly a casting material that is of course brass / bronze that is strong enough comparable to C67300?
The current part is cast c90300 bronze. We have had cracking issues in this part.
We have looked into a competitor part and the material they use is C67300 brass or CS33500, and possibly UNS 34000.
I'm looking into the basics and I'm trying to keep it as simple as possible, what do you look into to know what makes it stronger for high pressure applications. I found that the C90300 has a much lower Tensile and Yield strength rating compared to the two other materials I specified. Is is this something I can use to deterime a new material?
I'm just one of the drafter / designers here at this company and we do not have a engineer at the time for this type of work right now and I'm looking to you guys for help the first time. I have tried to search these fourms and I hope I found the proper location for this.
Some things I've noted on these types of material and found, C67300 is a typically forged type of material or bar round. I could assume that forging could be a big help for strength in the area we have the cracking issues at high pressure. And, is there possibly a casting material that is of course brass / bronze that is strong enough comparable to C67300?