Is anyone familiar with CAN/CSA-G40.21. I need to know how CAN/CSA-G40.21 Grade 300W for channels, angles and plates compares to an A36 designation. Does A36 meet the CAN/CSA-G40.21 Grade 300W requirements?
 
I haven't the info directly with me but as I believe (if memory serves) if the service temperature is < 250ºF then the two are equivalent, afterwards A36 diverges.

Today is gone. Today was fun.
Tomorrow is another one.
Every day, from here to there,
funny things are everywhere.
 
300W has a higher yield (44 ksi) than SA-36 (36 ksi). In my opinion, 300W is an overall stronger material. Anywhere SA-36 material is specified, 300W is generally an acceptable substitute (not necessarily every application). However, I would not automatically accept SA-36 in lieu of 300W due to the strength differences. Both are common grades of carbon steel. I have found the 300W very commonly used in Canada and SA-36 more commonly used in the United States. Also, in addition to the strength differences, there are minor chemistry differences. This link has a very brief comparison of the two.

 