Does anyone know where i can find an extensive guide to material selection? Thanks guys and gals
 
Replies continue below

Recommended for you

thryll, Check Perry's Chemical Engineer's Handbook, Section 23, "Materials of Construction".

Hope this helps.
saxon
 
Hello

My best choice for material selection is "Corrosion resistance tables" by Philip A. Schweitzer publich by Marcel Dekker inc. ISBN: 0-8247-8372-7.

It contain information on metals, nonmetals, coating, mortars,plastics, elastomers and lining.

I hope it will be helpfull to you.
 
Please refer the following references;

1) Metals Handbook : Volume13, Corrosion, ASM International
2) Corrosion Tables for Stainless Steels and Titanium, Jernkontoret, Sweden, 1979
3) Devereux, O.F., McEvily, A.J., Staehle, R.W., eds., Corrosion Fatigue, NACE-2, NACE, 1972
4) Fontana, M.G., Corrosion Engineering, McGraw-Hill, 1986
5) Gibala, R., and Hehemann, R.F., Hydrogen Embrittlement and Stress Corrosion Cracking, ASM International
6) Holmes, D.R., ed., Dew Point Corrosion, Ellis Horwood Ltd., 1985
7) Munger, C.G., Corrosion Prevention by Protective Coatings, NACE, 1985
8) Uhlig, H.H., Corrosion Handbook, John Wiley & Sons
9) Moniz, B.J. and Pollock. W.I., eds., Process Industries Corrosion : The Theory and Practice, NACE, 1986
10) NACE-2, Corrosion Fatigue, NACE, 1972
11) NACE-3, Localized Corrosion, NACE, 1974
12) Ohtani, R., Ohnami, M., and Inoue, T., High Temperature Creep-Fatigue, Elsevier Applied Science,1988
13) Parkins, R.N., Corrosion Prevention in the process Industries, NACE, 1990
14) Peckner, D., Bernstein, I.M., Handbook of Stainless Steels, McGraw-Hill Book Company, 1977
15) Sedriks, A.J., Corrosion of Stainless of Stainless Steels, John Wiley & Sons, 1979
16) Staehle, R.W., Brown, B.F., Kurger, J., Agrawal, A., eds., Localized Corrosion, NACE-3, NACE, 1974
17) Alberty, R.A., Physical Chemistry, John Wiley & Sons, 1983
18) Dieter, G.E., Mechanical Metallurgy, McGraw-Hill, 1976, MET
19) LaQue, F.L., Marine Corrosion : Causes and Prevention, John Wiley & Sons, 1975
20) Reed-Hill, R.E., Physical Metallurgy Principles, Prindle, Weber & Schmidt, 1973
21) Schweitzer, P.A., Corrosion and Corrosion Protection Handbook, Marcel Dekker, Inc., 1983
22) Shreir, L.L., ed., Corrosion, John Wilery & Sons, 1963
23) Smith, W.F., Structure and Properties of Engineering Alloys, McGraw-Hill, 1981
24) Szklarska-Smialowska, Z., Pitting Corrosion of Metals, NACE. 1986
25) NACE, Corrosion Data Survey
26)Uhlig, H.H., Corrosion and Corrosion Control, An Introduction to Corrosion Science and Engineering, John Wiley & Sons, Inc., 1985

[Attention]
Do not make a decision with only one reference because there are diverse data, mechanism, and countermeasures for the same/similar situation.

NACE Materials Selection/Design and Corrosion Specialist
 
thank you for all of this information
 