I am curious why G12150 is not an approved material listed in Sec II part D? Does it have to do with it being resulfurized?
 
Replies continue below

Recommended for you

ASME uses the ASTM material base. The Code does provide for some exceptions. See ASME SecVIII Div1 UG-4,UG-10,UG-15.
 