I am cuently working on a North sea Project which I inhereted a couple of months ago. In somebodys wisdom they decided to use two housings made from ST-ST which at temperature mate and Gall the threads. Has anybody any Ideas on alternative materials I may use possibly self lubricating to avoid the two housings galling, yet holding the same material properties of 17-4 PH ST-ST H150-M
HRC = 27-33
min yield = 75 ksi
min tensile = 115 ksi
I have looked at a number of materials but help would be gratefully recieved cheers
HRC = 27-33
min yield = 75 ksi
min tensile = 115 ksi
I have looked at a number of materials but help would be gratefully recieved cheers