material selection of pump 3

Status
Not open for further replies.

Salghetet

Materials
Jul 11, 2011
22
Ladies and Gentlmen
we have corrosion problem with pump used for treated water in industrial area
material of wet pump is carbon steel and cast iron (casing, impellar and shaft)
i want to upgrade material of vertical Aerator Effluent Pump
i am thinking about nonmetallic material or steel lined with PTFE or SS
so please advise if you have experience
 
Replies continue below

Recommended for you

Plastic will be the best choice concerning corrosion and cheaper than stainless steel or any lined metal. Talk to companies like Goulds, Grundfos or Grainger. They should be able to help.
 
what about temperature damage and mechanical damage of impellar and shaft due to rotating if material is plastic
 
Rubber lined pumps can be an alternative. Pump shafts are commonly made in 400 series or 17-4 PH stainless steels.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
400 series or 17-4 PH stainless steels are good for high temperature above 200C but in our case temperature is normal will not exceed 80C
 
water is oily treated water from effluent area of LNg plant
 
Or, depending on the pump size, Ni-Resist may be an option. The alloy is more expensive but casting and finishing are less costly than with SS. This is a very proven alloy in bad water service.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Are there certain types of plastic that we should look for if we have, say, an alkaline cleaner for a passivation cleaning? This thread is suddenly becoming extremely relevant IRL.
 