I am designing a type of muzzle break for small arms. One part of the brake will be directly impinged upon by the hot, erosive muzzle blast after the projectile has left the barrel.
I am looking for material suggestions. I am considering Inconel but was wondering if there might be some other, easier to machine material options.
TIA
I am looking for material suggestions. I am considering Inconel but was wondering if there might be some other, easier to machine material options.