Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

material selection in sulfuric acid

Status
Not open for further replies.

ras85

Materials
Joined
Feb 9, 2012
Messages
28
i need to select material for pump shaft in sulfuric acid at 98% concentration and 120 C. i would like to know any one has experience on chrome plating coating on this application or maybe kindly suggest another solution.
 
First off; review information on pumps suitable for sulfuric acid service


Second, review information on suitable materials and the effects of velocity. Ni-base alloy would be required given flow induced effects on material performance and 120 deg C.

Third, chrome plating would not be recommended for this application.
 
thanks, its so helpful!
 
Get a hold of the MTI Material Selector series MS-1.
It is the best Sulfuric guide that there is.

= = = = = = = = = = = = = = = = = = = =