Jun 28, 2000 #1 alanb Mechanical Joined May 25, 2000 Messages 2 Location US Hi,<br><br>I have to design some dipping tanks to hold 96% sulfuric acid at 194 degrees F. Any ideas on materials, bearing in mind that cost is an issue too?<br><br>Thanks,<br><br>Alan B
Hi,<br><br>I have to design some dipping tanks to hold 96% sulfuric acid at 194 degrees F. Any ideas on materials, bearing in mind that cost is an issue too?<br><br>Thanks,<br><br>Alan B
Sep 20, 2000 #2 snafi Mechanical Joined Aug 7, 2000 Messages 1 Location SA Hi, I know that my answer is may be too late but it might be helpful for others. Try (ZeCore) material it is cheaper than Sandvik SX and has very good corrosion resistance to Acid at this Temp. [sig][/sig] Upvote 0 Downvote
Hi, I know that my answer is may be too late but it might be helpful for others. Try (ZeCore) material it is cheaper than Sandvik SX and has very good corrosion resistance to Acid at this Temp. [sig][/sig]