I need some information, kindly provide:
what material of tank / vessel is recommended for the storage of liquid nitrogen.The expected Min. Design Temperature would be -320 Deg F.
One option is stainless. 304L is used for a lot of crygenic applications. There is a large CTE to work with, but there is no ductile/brittle trasition to worry about.
= = = = = = = = = = = = = = = = = = = =