ASME B16.34 is for Valves, Flanged, Threaded, and Welding End.
The materials group 1.1 listed in this code is for carbon steel materials which "may" be acceptable in the appropriate pipe code.
however, it is best to investigate the scope diagrams in B31.8 or B31.3 for appropriate use.
my guess would be B31.8.