Jan 7, 2003 #1 toeng Mechanical Joined Jan 7, 2003 Messages 1 Location CA Does anyone now what the following material callout is S45CVS1 :-}
Jan 13, 2003 1 #2 GearmanPE Mechanical Joined Dec 18, 2002 Messages 38 Location US toeng ; I found reference to S45C, which is a Japan grade approximatly equal to SAE 1045. Upvote 0 Downvote