Material S45CVS1 1

Status
Not open for further replies.

toeng

Mechanical
Jan 7, 2003
1
Does anyone now what the following material callout is

S45CVS1


:-}



 
Replies continue below

Recommended for you

toeng ;
I found reference to S45C, which is a Japan grade approximatly equal to SAE 1045.
 