Where can I find the material properties of SA-105, SA-182-316 and SA-182-304 at various temperature, in particular 316 stainless steel forgings at 850 deg. F?

Elastic Modulus
Poisson's Ratio
Shear Modulus
Mass Density
Tensile Strength
Yeild Strength
 
Replies continue below

Recommended for you

For these ASME materials, you can find most of this information in ASME Section II, Part D, Table for UTS, YS and Subpart 2 on Physical Properties.
 