Hello,
I am in the process of doing an FEA on a part made out of G-10. I am unable to find some material properties that are necessary for the FEA. I have some of the standard stuff, tensile strength, Modulus of Elasticity etc, but I cannot find any information about Poisson ratio.

I have checked all of my regular sources, and some textbooks.

Can anyone point me to a source for this info? Can anyone explain why the poisson is not listed for G-10?

-Shaggy
 
If memory serves me G10 is a laminate commonly used for knife-scales, among other things. Since it's a glass reinfroced epoxy, can you find estimates? Also, can you find any data for the trade name Micarta?
 
On second thought, I don't believe Micarta is a trade name. Oh also, can you find anything for FR4?
 