Material properties of 302 stainless steel 25% hardened

Status
Not open for further replies.

jbigelow

Automotive
Jul 19, 2006
7
I was wondering if anybody had a material curve for 302 stainless steel 25% hardened?
Or at least the n, r, K value.
 
Replies continue below

Recommended for you

For 302 stainless steel, mechanical properties

1/4 hard;
125-150 Ksi UTS
75 Ksi min yield
10% min Elongation (2" gage)
 