Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

material properties at cryogenic temperatures 1

Status
Not open for further replies.

jollyholly

Materials
Joined
Jan 5, 2009
Messages
2
Location
US
hello,
I am trying to find electrical and thermal properties of materials such as alumina, titania, and various metal oxides at 4K and 77K. I have scoured the internet trying to find the properties and have gone to a major university library without success. Any help or resources that you know of would be greatly appreciated.
Thank you!
 
Hi jolly,
The only references that summarize various material properties under cryogenic conditions that I have only cover the typical metals and plastics. Here's a couple I have excerpts from that you might try:
Thermophysical properties of matter by Y. S. Touloukian and C. Y. Ho
also,
Materials at Low Temperatures by Richard P. Reed and Alan F. Clark
You might look for these in a local university library.

Otherwise, I'd suggest doing a Google Scholar search for specific papers. For example: "Dielectric Properties of Single Crystals of Al2O3, LaAlO3, NdGaO3, SrTiO3, and MgO at Cryogenic Temperatures" by Jerzy Krupta et al.
 