Chrome-silicon alloy steel wire ASTM A401
Field of use of the selected material
Suitability for fatigue load Very good
Relative strength High
Corrosion resistance Poor
Max. operational temperature - 475 [° F]
Delivered wire diameters / 0.031 - 0.5 [in]
Mechanical and physical properties of the material
Modulus of elasticity in shear – 11200 [ksi]
Modulus of elasticity in tension – 28500 [ksi]
Density - 490 [lb/ft3]
Strength characteristics of the material
Ultimate tensile strength / Su - 260 [ksi]
Permissible torsional stress tA / 166.4 [ksi]
Endurance limit in shear te / 96.2 [ksi]
Endurance limit by finite life tf / 96.2 [ksi]
Mirekp
Mechanical and engineering calculations