Jack1_2-3_4-5_

Materials
Dec 20, 2016
8
Hello

I am designing a tool holder for a motorcycle, that will come in contact with many chemicals on and around the motorcycle.
I have selected HDPE to manufacture it out of injection moulding.
Is there any other materials (plastic) that I could use.??? [smile2][smile2]
 
Replies continue below

Recommended for you

I would look at glass filled nylons.

----------------------------------------

The Help for this program was created in Windows Help format, which depends on a feature that isn't included in this version of Windows.
 
Actually I think you could try PP too. It is widely used to produce this kind of box/case in China. ABS is expensive, while PE is not so tough like PP.

Expert of nucleating agents
 