I am helping develop a spreadsheet for calculating probe conformity with ASME PTC-19.3 2014.
Can someone point me in the right direction for finding the associated standard/s that will give us Young's Modulus Data and Density figures?
We have the tensile/yield data from the material standards, but the above information is not included in the material standards that we have (although I am sure it is one of the associated reference standards)

Would a reference such as the Metals Handbook provide all of the above?

The materials we are looking at using including are :
ASTM A182 F316/316L
ASTM A269 316/316L
ASTM A276 316/316L
ASTM A276 2205
ASTM A276 2507
ASTM A182 F51
ASTM A312 316/316L

Appreciate any help in pointing us in the right direction.
Thanks!
 
Do you have a copy of the B&PVC?
There are tables of physical properties in the Code.
You can find such info in the Metals Handbook.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Thanks Ed.
I do have a copy of AS1210 which is the Australian B&PVC. Don't know why I didn't think of looking in there!
It has the E figures for 316 which is great, doesn't cover off the 2205/2507/F51 though.
Will consider getting hold of the Metals Handbook if it covers these (and other materials we haven't used yet)
Appreciate the push in the right direction!
 
For 2205 and 2507 I would trust the numbers published by Outokumpu in their literature.
F51 is 2205 by another name.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
That's what we have done in the past (quoting manufacturers numbers).
Our preference this time around would be to reference standards where we can.
 
Outokumpu has been making duplex stainless a long time.
Trust their data.
These are newer alloys and there isn't a lot of bad older data out there (like there is for 316).

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Temperature dependent E-numbers are found in ASME II-D, subpart 3, figure HA-5.
 