Hello everyone,
Currently I am investigating the crush behavior of thin walled tubes. Therefore I am doing some analysis with ANSYS/LS-Dyna.
I have a brief question concernen the Material Model 24 (Piecewise Linear Plasticity):
First of all I have obtained a true stress vs. true strain curve for my material (AA6060 T6). Since I have to insert a effective plastic strain vs. effetive stress curve I have transformed it by subtracting true_stress/E. It wasnt excatly 0, thats why I have subtracting the remaining strain as a constant factor from the curve, so that it starts at 0. I hope my method is correct so far. The problem is, that the true stress vs. true strain curve is only defined up to the point of ultimate stress. Does it make sense to assume a perfect plastic behaviour after this point or is it better to extrapolate the remaining curve e.g. with the Voce-Equation? I have compared both results and the results with the voce equation show a way more ductile behavior for some reason.
Does anyone know some advice for me? In papers und in literature the insertion of the material data is not properly explained.
Thanks in advance for your help!
Ed93
Currently I am investigating the crush behavior of thin walled tubes. Therefore I am doing some analysis with ANSYS/LS-Dyna.
I have a brief question concernen the Material Model 24 (Piecewise Linear Plasticity):
First of all I have obtained a true stress vs. true strain curve for my material (AA6060 T6). Since I have to insert a effective plastic strain vs. effetive stress curve I have transformed it by subtracting true_stress/E. It wasnt excatly 0, thats why I have subtracting the remaining strain as a constant factor from the curve, so that it starts at 0. I hope my method is correct so far. The problem is, that the true stress vs. true strain curve is only defined up to the point of ultimate stress. Does it make sense to assume a perfect plastic behaviour after this point or is it better to extrapolate the remaining curve e.g. with the Voce-Equation? I have compared both results and the results with the voce equation show a way more ductile behavior for some reason.
Does anyone know some advice for me? In papers und in literature the insertion of the material data is not properly explained.
Thanks in advance for your help!
Ed93