brandonb73
Mechanical
Our client has a pressure vessel in which was installed an unauthorized nozzle. The State has told them the nozzle can stay persuant to an acceptable UT test and calculations showing the material thickness is adequate.
The customer has provided a spectrochemical analysis of the material. In order to run calculations however, I need tensil and yield strength data. Do I need to ask the customer to also have these test done or is there some way to obtain this based on the spectrochemical analysis?