radixeng

Civil/Environmental
Sep 20, 2012
2
Good day folks,


We are looking to fabricate a support stand for a tote bin containing caustic material.

I'm looking into the use of Alloy 20 for the support stand but of course the cost might be of the charts.

Can anyone provide some suggestions on materials which we can use to bear the sulfuric acid?

Any information provided will be greatly appreciated.

Thanks.
 
Replies continue below

Recommended for you

"Caustic" is usually used for bases, not acids.

Check into fiberglass, maybe?
 