I would be more inclined to 50% GF nylon.
I have seen some testing done many years ago, so I have forgotten a lot of the details, but as I recall 50% GF 66 was best, but there was not much difference between 6 and 6.6 at 50% glass. The 6 is somewhat easier to mould.
50% GF 6 is also currently used for plasterboard screws.
If it will bear the cost, 50% long glass fibre 6.6 will give even better performance, but it is expensive, and it requires some care with machine and mould details.
Regards