The piping classes are Duplex SS and Super Duplex SS. Can we use SS316 tubing for instruments as DSS/SDSS tubing are not available in market and the next higher grade for tubing available in market is Inconel 625 which is not locally available and will cost heavily.
Service is water injection with high chlorides and also hydrocarbon with H2S and chlorides.
Note: Instrument tubing discussed are only used to drain the fluid when DBB valves are opened. These are connected to the flanges and are used with instruments suchas pressure gauges.