A client has asked us to manufacture a helical type cooler which is submerged in an aqueous solution of 11% sulfuric acid and 25% sodium chloride, at 55 °C. Initially, the client proposed to manufacture the tubes with CP titanium, however I have some doubts about their resistance considering the concentration of sulfuric acid. Another alternative we are considering is alloy 825. Could someone give me some help or advice about it?
Thanks
Thanks