Dear everyone,
With reference to datasheet for deaerator storage drum, SS 316L cladding is required for deaerator storage drum.
my deaerator storage drum's condition is as follows:
- Temp.: 115 degree C
- Press.: 0.7 bar
- controled pH: 8.5 ~ 9.5 @ 25 degree C
- Oxygen Control: 7 bbp
CS + 3.0 mm CA have been applied as per our experience same as above condition).
However, I don't have any reference for persuading to change the material.
would you recommended any kind of reference for material change from SS to CS? Or SS is suitable?
With reference to datasheet for deaerator storage drum, SS 316L cladding is required for deaerator storage drum.
my deaerator storage drum's condition is as follows:
- Temp.: 115 degree C
- Press.: 0.7 bar
- controled pH: 8.5 ~ 9.5 @ 25 degree C
- Oxygen Control: 7 bbp
CS + 3.0 mm CA have been applied as per our experience same as above condition).
However, I don't have any reference for persuading to change the material.
would you recommended any kind of reference for material change from SS to CS? Or SS is suitable?