material for collets

Status
Not open for further replies.

idanbrk

Mechanical
Jun 23, 2014
20
hi,

can anyone tell me what material is used to make collets? if there is more then one option its even better
 
Replies continue below

Recommended for you

its probably a spring steel, but in searching 65MN comes up alot, this is probably the majority.
 
You can use a variety of materials, depending upon the intended application. Case carburized, hardened and tempered AISI 8620 is a fairly common steel used for manufacturing collets. Spring steel grades such as AISI 6150 are also commonly used for manufacturing collets. I have even made them out of aluminum for certain applications with success.

Maui

 