Material equivalent

Status
Not open for further replies.

bruv

Materials
Joined
Feb 19, 2002
Messages
239
Location
GB
Can anybody please tell me the nearest forged equivalent to cast ASTM A216 WCB? I'm not worried if you provide US or European specifications.

Thanks
 
The nearest ASTM specifications are A-105 and A-181

 
Can anyone direct me to a cross-reference from JIS to AISI steels? Thanks!
 