Dec 4, 2003 #1 MW76 Structural Joined Dec 10, 2002 Messages 8 Location TN COULD YOU PLEASE HELP ME TO DEFINE THIS MATERIAL: C 35 N (DIN) WHAT THAT MEANS "N" WHAT IS THE MINIMAL STRENTH REQUIRED THANK YOU IN ADVANCE
COULD YOU PLEASE HELP ME TO DEFINE THIS MATERIAL: C 35 N (DIN) WHAT THAT MEANS "N" WHAT IS THE MINIMAL STRENTH REQUIRED THANK YOU IN ADVANCE
Dec 4, 2003 #2 aviat Aerospace Joined Oct 13, 2003 Messages 269 Location CA Normalized http://www.dalmine.it/dal_portal2002/it/pdf/prodotti/meccanica/meccaniciFreddo_en.pdf Upvote 0 Downvote