For a 1000psi autoclave you want the long term risk of embrittlement to be nil, not just low.
That is why these are usually made from Ni alloys such as 625.
They also are usually designed with higher safety factors, such as 5 to 1.
1000 gal is a large volume at that pressure, play it safe.
We used small ones, about 1gal. They were 316L and were designed at 6 to 1 SF.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube